发明名称 コークスの製造方法
摘要 PROBLEM TO BE SOLVED: To provide a method for producing coke, in which a coal blend, that contains poor-quality coal at the least and is used for molded coal, is pulverized, a binder is added to the pulverized coal blend, the binder-added coal blend is kneaded, the kneaded coal is molded in a molding machine to obtain molded coal, the molded coal is charged into a coke oven together with the powdered coal prepared by pulverizing another coal blend for coal powder and the charged coal is dry-distilled and in which the coke having high strength can be produced stably even when the amount of the poor-quality coal to be blended in the molded coal is increased.SOLUTION: The weighted average of the total expansion coefficient, which is obtained by calculating a weighted average of the total expansion coefficient of the coal to be blended in the coal blend for molded coal, is defined as &Sgr;TD and a ratio of coal particles, which are obtained by pulverizing the coal blend for molded coal and each of which has 3 mm or smaller particle diameter, is defined as RD. When &Sgr;TD is lower than 40%, the coal blend for molded coal is pulverized to produce the molded coal so that RD becomes 75-95 mass% and when &Sgr;TD is 40-60%, the coal blend for molded coal is pulverized to produce the molded coal so that RD becomes 95 mass% or lower.
申请公布号 JP5942971(B2) 申请公布日期 2016.06.29
申请号 JP20130260496 申请日期 2013.12.17
申请人 新日鐵住金株式会社 发明人 渡邉 雅彦;上坊 和弥;窪田 征弘
分类号 C10B57/04;C10B53/08 主分类号 C10B57/04
代理机构 代理人
主权项
地址