A tempered glass according to one embodiment of the present invention is a tempered glass having a compression stress layer in a surface thereof, the tempered glass including as a glass composition, in terms of mass %, 45 to 75% of SiO2, 10 to 25% of Al2O3, 0 to 10% of B2O2, 0 to 8% of MgO, 0 to 20% of SrO+BaO, and 0 to 14% of Na2O. Herein, the term “SrO+BaO” refers to the total amount of SrO and BaO. |