发明名称 |
FAST FIRING METHOD FOR HIGH POROSITY CERAMICS |
摘要 |
A method for firing a green honeycomb ceramic body including heating the green honeycomb ceramic body from room temperature to a first temperature of about 300° C. The green honeycomb ceramic body is then heated from the first temperature to a second temperature of greater than or equal to about 800° C. at a heating rate of greater than or equal to about 90° C./hr. The green honeycomb ceramic body may have a diameter of from greater than or equal to about 4.0 inches to less than or equal to about 9.0 inches, and it may include a carbon-based pore former in a concentration of from greater than or equal to about 10% to less than or equal to about 45% by weight. |
申请公布号 |
EP3024798(A1) |
申请公布日期 |
2016.06.01 |
申请号 |
EP20140750648 |
申请日期 |
2014.07.23 |
申请人 |
CORNING INCORPORATED |
发明人 |
BRONFENBRENNER, DAVID, JACK;IYER, SRIRAM, RANGARAJAN |
分类号 |
C04B35/00;C04B35/195;C04B35/626;C04B38/00 |
主分类号 |
C04B35/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|