发明名称 カーボンナノチューブを含有するビニロン繊維およびその製造方法
摘要 PROBLEM TO BE SOLVED: To provide a vinylon fiber having unevenness on a surface and a method for producing the same, and also to provide a carbon nanotube aggregate produced by using the vinylon fiber and a method for producing the same.SOLUTION: The method for producing a vinylon fiber includes a step of fiberizing a spinning dope by a wet spinning method. The spinning dope contains a polyvinyl alcohol-based polymer, a carbon nanotube and water and has a thixotropy index (TI) of 2.1-3.0, which is a ratio of the viscosity at a shear rate of 10(1/sec.) to the viscosity at a shear rate 100(1/sec.) which are measured by using a conic-plane rotational viscosimeter under a condition of temperature 25°C.
申请公布号 JP5919018(B2) 申请公布日期 2016.05.18
申请号 JP20120028968 申请日期 2012.02.13
申请人 ニッタ株式会社;ユニチカ株式会社 发明人 中井 勉之;小向 拓治;吉原 久美子;稲垣 孝司;小嶋 富夫;漆崎 学
分类号 D01F6/50;B82Y30/00;B82Y40/00;C01B31/02;D01F9/127 主分类号 D01F6/50