发明名称 WET PROCESS FOR SMELTING NICKEL OXIDE ORE
摘要 A process for smelting that can attain a high leaching ratio of nickel and cobalt and a high oxidation ratio of iron to trivalent iron, and, at the same time, can reduce energy cost by suppressing the amount of high-pressure air to be used as an oxidant and the amount of high-pressure steam to be used for maintaining temperature. In a smelting method comprising a first step for slurrying nickel oxide ore and a second step for adding sulfuric acid to the ore slurry and leaching the ore slurry while blowing high-pressure air and high-pressure steam therein, characterized by adjusting the carbon grade in a solid content of ore slurry so as to be 0.1 to 0.5% by mass depending on the blending ratio of the nickel oxide ore that constitutes the ore slurry in the first step and controlling oxidation-reduction potential (Ag/AgCl basis) of the leachate to 400 to 600 mV by adjusting the amount of the high-pressure air to be blown so as to be 700 to 800 Nm3 per ton of carbon in a solid content of ore slurry in the second step.
申请公布号 CA2650372(C) 申请公布日期 2016.05.03
申请号 CA20092650372 申请日期 2009.01.21
申请人 SUMITOMO METAL MINING CO., LTD. 发明人 SHIBAYAMA, KEISUKE;OZAKI, YOSHITOMO;NAKAI, OSAMU
分类号 C22B23/06;C22B1/00;C22B3/08;C22B23/00 主分类号 C22B23/06
代理机构 代理人
主权项
地址