摘要 |
PROBLEM TO BE SOLVED: To provide a laminate comprising a resin sheet and a fiber sheet, which is excellent in insulation properties and interlayer adhesive property.SOLUTION: There is provided a laminate obtained by laminating a fiber sheet on at least one surface of a resin sheet, where the total thickness of the laminate is 50 to 100 μm, the ratio of the dielectric breakdown voltage (kV)/the whole thickness of the laminate (μm) is 0.080 to 0.150 kV/μm and the stress-strain curve in the tensile test of the laminate has no minimum points.SELECTED DRAWING: None |