PROBLEM TO BE SOLVED: To provide an ethylenic polymer composition for a thin-walled container, which has excellent moldability, durability and impact strength, hardly causes unevenness derived from a high-molecular weight gel and which enables a molded article having excellent appearance to be produced, and also to provide a molding made of the ethylenic polymer composition.SOLUTION: There is provided the ethylenic polymer composition containing 10 to 90 wt.% of the ethylenic polymer (D) having a density of 0.900-0.975 g/cmand a melt flow rate of 0.05-1,000 g/10 min, and 90 to 10 wt.% of an ethylenic polymer (C) obtained by the multi-stage polymerization of the components (A) and (B), where the component (A) is an ethylenic polymer having a density of 0.900-0.950 g/cmand a high load melt flow rate of 0.1-100 g/10 min; and the component (B) is another ethylenic polymer having a density of 0.900-0.970 g/cmand a high load melt flow rate of 0.5-1,000 g/10 min.SELECTED DRAWING: None |