发明名称 METHOD FOR MANUFACTURING A TITANIUM-ALUMINIUM ALLOY PART
摘要 A method manufactures a metal alloy part by spark plasma sintering. The method includes the simultaneous application, inside a die, of a uniaxial pressure and of an electric current to a powder component material that has the following composition: 42 to 49% aluminum, 0.05 to 1.5% boron, at least 0.2% of at least one element selected from tungsten, rhenium and zirconium, optionally 0 to 5% of one or more elements selected from chromium, niobium, molybdenum, silicon and carbon, the balance being titanium and the total of the elements without aluminum and titanium being between 0.25 and 12%.
申请公布号 EP3007844(A1) 申请公布日期 2016.04.20
申请号 EP20140734884 申请日期 2014.06.11
申请人 CENTRE NATIONAL DE LA RECHERCHE SCIENTIFIQUE (C.N.R.S.);OFFICE NATIONAL D'ETUDES ET DE RECHERCHES AÉROSPATIALES (ONERA) 发明人 COURET, ALAIN;MONCHOUX, JEAN-PHILIPPE;THOMAS, MARC;VOISIN, THOMAS
分类号 B22F3/14;B22F3/105;B22F5/04;C22C1/04;C22C14/00;C22F1/18;F01D5/28;F01L3/02 主分类号 B22F3/14
代理机构 代理人
主权项
地址