摘要 |
A method for the continuous production, at high polymerization yield, of an oxymethylene copolymer having improved thermal stability and formaldehyde emission, while maintaining toughness and rigidity, is provided. Provided is a production method for oxymethylene copolymer, including: a step of carrying out a copolymerization reaction of trioxane and 1,3-dioxolane in an amount of 0.9-2.4 mass% with respect to the trioxane, in the presence of 0.001-0.007 mol% of boron trifluoride and 0.006-2.0 mass% of a sterically hindered phenol with respect to the trioxane; and a step of adding a polymerization terminator to the reaction system at the point in time that the polymerization yield of the copolymerization reaction has reached 92% or above, to terminate polymerization. |