发明名称 |
Temperature-resistant silicone resins |
摘要 |
Methods and formulations for modified silicone resins of Formula (I) are presented:;
The R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher). |
申请公布号 |
US9309359(B2) |
申请公布日期 |
2016.04.12 |
申请号 |
US201414329885 |
申请日期 |
2014.07.11 |
申请人 |
The Boeing Company |
发明人 |
Zhou Chaoyin;Nowak Andrew P.;Sharp Richard E.;Li Wen;French James E. |
分类号 |
C08L83/04;C08G77/04;C08G79/04;C08G77/58;C08K3/22;C08L85/02;C08G77/00;C08G77/20 |
主分类号 |
C08L83/04 |
代理机构 |
Patterson & Sheridan, LLP |
代理人 |
Patterson & Sheridan, LLP |
主权项 |
1. A modified silicone resin of Formula (I): wherein R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000;wherein the resin of Formula (I) has a viscosity ranging from about 500 cSt to about 10,000 cSt. |