发明名称 |
PREPARATION METHOD FOR POLYOLEFIN POLYMER FOR FIBER PRODUCTION |
摘要 |
The present invention relates to: a polyolefin which exhibits narrow molecular weight distribution, high strength and a high stretching ratio; and a preparation method therefor. According to the present invention, it is possible to provide polyethylene with high catalyst activity, high molecular weight, and controlled molecular weight distribution by using, in polymerization of an olefin monomer, a hybrid metallocene supported catalyst in which a borate compound is used as a second co-catalyst. In addition, if the polyolefin is processed, it is possible to produce a fiber with excellent mechanical properties and an excellent stretching ratio. |
申请公布号 |
WO2016052982(A1) |
申请公布日期 |
2016.04.07 |
申请号 |
WO2015KR10296 |
申请日期 |
2015.09.30 |
申请人 |
LG CHEM, LTD. |
发明人 |
LEE, SEUNG MI;HONG, DAE SIK;SONG, EUN KYOUNG;KWON, HEON YONG;YOU, YOUNG SUK;LEE, KI SOO;SONG, KI HEON |
分类号 |
C08F4/6592;C08F4/12;C08F4/64;C08F10/00 |
主分类号 |
C08F4/6592 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|