Anion binder for solid alkaline fuel cell, method of preparing the same and membrane-electrode assembly |
摘要 |
The present invention concerns the preparation of an anion binder for a solid alkaline fuel cell which enhances durability to electrochemical reactions and makes the production of electrode slurry easy. A method of preparing an anion binder for a solid alkaline fuel cell includes: (A) mixing an electrolytic monomer of quaternary ammonium salts having a cation group, a bisacrylicamide crosslinking agent having a tertiary amino group, and water together by stirring; (B) mixing the mixture with a photoinitiator; (C) interposing the solution between polyethylene terephthalate films and irradiating the solution with ultraviolet light for crosslinking and polymerization; and (D) pulverizing crosslinked polymerized resin to a nano size. |
申请公布号 |
US9306233(B2) |
申请公布日期 |
2016.04.05 |
申请号 |
US201313924840 |
申请日期 |
2013.06.24 |
申请人 |
KOREA INSTITUTE OF ENERGY RESEARCH |
发明人 |
Choi Young Woo;Lee Mi Soon;Yang Tae Hyun;Kim Chang Soo;Yoon Young Gi;Park Seok Hee;Yim Sung Dae;Park Gu Gon;Sohn Young Jun;Kim Minjin;Bae Byungchan |
分类号 |
H01M8/02;H01M8/10;H01M8/08;H01M4/86 |
主分类号 |
H01M8/02 |
代理机构 |
Galgano IP Law PLLC |
代理人 |
Galgano IP Law PLLC ;Galgano Thomas M.;McDonald Jessica G. |
主权项 |
1. A method of preparing an anion binder for a solid alkaline fuel cell, the method comprising:
(A) mixing an electrolytic monomer of quaternary ammonium salts having a cation group, a bisacrylicamide crosslinking agent having a tertiary amino group, and water together by stirring; (B) mixing the mixture with a photoinitiator; (C) interposing the solution between polyethylene terephthalate films and irradiating the solution with ultraviolet light for crosslinking and polymerization; and (D) pulverizing crosslinked polymerized resin to a nano size, wherein (D) comprises:
(D1) primarily pulverizing the crosslinked polymerized resin to a size of 40 to 60 μm by a grinding pulverizer; and(D2) dispersing and secondarily pulverizing the powder obtained in the primary pulverization to a size of 150 to 250 nm by a wet pulverizer. |