发明名称 焼結助剤を用いた溶剤系耐環境コーティングの製造方法
摘要 A method for making an environmental barrier coating (12) using a sintering aid comprising: combining at least an organic solvent, and a primary transition material comprising a rare earth disilicate, or a doped rare earth disilicate to produce a transition layer slurry; combining at least an organic solvent, and a primary outer material comprising a rare earth monosilicate or a doped rare earth monosilicate to produce an outer layer slurry; combining at least an organic solvent, and a primary compliant material comprising BSAS or a rare earth doped BSAS to produce a compliant layer slurry; applying at least the transition layer slurry, and any one or more of the outer layer slurry or the compliant layer slurry, to a component (10); infiltrating a sol-gel solution comprising an aqueous solution of a water soluble salt sintering aid, or an organic solvent solution of a solvent soluble salt sintering aid into the applied slurry layers; and sintering the component (10) to produce the environmental barrier coating having at least a transition layer (16) and any one or more of an outer layer (20) or a (18) compliant layer wherein during sintering a reaction between the primary materials and the sintering aid results in the transition layer comprising a porosity of from 0% to about 15% by volume of the transition layer, the outer layer comprising a porosity of from 0% to about 30% by volume of the outer layer, and the compliant layer comprising a porosity of from about 0% to about 30% by volume of the compliant layer.
申请公布号 JP5890957(B2) 申请公布日期 2016.03.22
申请号 JP20100169935 申请日期 2010.07.29
申请人 ゼネラル・エレクトリック・カンパニイ 发明人 グレン・ハロルド・カービイ;ブレット・アレン・ボウトウェル
分类号 C04B41/85;C04B41/89;F01D5/28;F01D25/00;F02C7/00;F23R3/42 主分类号 C04B41/85
代理机构 代理人
主权项
地址