发明名称 Process for improving the mechanical and processing properties of linear high polymers of propylene
摘要 A crystallizable, linear head-to-tail high polymer of propylene is subjected to thermal degradation until the average degree of polymerization has been reduced to such an extent that on the completion of production of articles by a forming process involving heating the average degree of polymerization will have been reduced to a value corresponding to an intrinsic viscosity, measured in tetrahydronaphthalene at 135 DEG C., of from 0.8 to 1.8. The thermal degradation may be effected by heating at 250-350 DEG C. in the absence of oxygen or at 150-180 DEG C. in the presence of oxygen. A stabilizer may be present during the degradation or added at the end of the treatment. Up to 30% of amorphone polypropylene may be present with the crystallizable polymer. The product may be filamentary or laminar, and may be extrusion- or injection-moulded or calendered. Specifications 810,023 and 828,791 are referred to.
申请公布号 GB835038(A) 申请公布日期 1960.05.18
申请号 GB19560036349 申请日期 1956.11.28
申请人 MONTECATINI SOCIETA GENERALE PER L'INDUSTRIA MINERARIA E CHIMICA 发明人
分类号 C08F8/50;C08K5/00 主分类号 C08F8/50
代理机构 代理人
主权项
地址