发明名称 配向性MAX相セラミック及びその製造方法
摘要 An oriented ceramic containing an Mn+1AXn phase, where the Mn+1AXn phase is a ternary compound, and M is an early transition metal, A is an A group element, X is C or N, and n is an integer of 1 to 3, wherein the oriented ceramic has a layered microstructure similar to shell layers of pearl, which is formed by laminating a layer of a nano-order to milli-order in a thickness thereof, and the oriented ceramic is an oriented bulk material a total thickness of which is in milli-order or larger at smallest.
申请公布号 JP5881174(B2) 申请公布日期 2016.03.09
申请号 JP20120512813 申请日期 2011.04.22
申请人 国立研究開発法人物質・材料研究機構 发明人 フ ショーフェン;グラッソ サルバトーレ;目 義雄;田中 英彦;鈴木 達
分类号 C04B35/56;C04B35/58 主分类号 C04B35/56