STRESS-CRACK-RESISTANT, HALOGEN-FREE, FLAME-PROTECTED POLYESTER |
摘要 |
1. The invention relates to the use of polyester molding compositions composed of
A) from 20 to 97.9% by weight of a thermoplastic polyesterB) from 0.1 to 10% by weight of an epoxidized natural oil or fatty acid ester, or mixture of these, where the epoxide equivalent weight of component B) in accordance with DIN EN ISO 3001 is from 100 to 400 g/eqC) from 1 to 20% by weight of a metal salt of a phosphinic acidD) from 1 to 20% by weight of a melamine compoundE) from 0 to 60% by weight of other additional substances,where the total of the percentages by weight of components A) to E) is 100%, for the production of stress-cracking-resistant and halogen-free flame-retardant polyester molding compositions. |
申请公布号 |
US2016060431(A1) |
申请公布日期 |
2016.03.03 |
申请号 |
US201414786177 |
申请日期 |
2014.04.15 |
申请人 |
BASF SE |
发明人 |
Roth Michael;Uske Klaus;Wagner Sebastian;Wolf Ulli |
分类号 |
C08K5/5313;C08K5/1515;C08K5/3492 |
主分类号 |
C08K5/5313 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method of producing a stress-cracking-resistant and halogen-free flame-retardant polyester molding comprising the use of polyester molding compositions comprising
A) from 20 to 97.9% by weight of a thermoplastic polyester B) from 0.1 to 10% by weight of an epoxidized natural oil or fatty acid ester, or mixture of these, where the epoxide equivalent weight of component B) in accordance with DIN EN ISO 3001 is from 100 to 400 g/eq C) from 1 to 20% by weight of a metal salt of a phosphinic acid D) from 1 to 20% by weight of a melamine compound E) from 0 to 60% by weight of other additional substances, where the total of the percentages by weight of components A) to E) is 100. |