摘要 |
<P>PROBLEM TO BE SOLVED: To provide a high toughness, high strength mortar composition which early develops high toughness and high compressive strength only by usual curing even at low temperatures. <P>SOLUTION: The high toughness, high strength mortar composition includes cement, ultra-fine slag, a water reducing agent, a defoaming agent, and fine aggregate. The Blaine specific surface area of the ultra-fine slag is 10,000-20,000 cm<SP POS="POST">2</SP>/g. <P>COPYRIGHT: (C)2012,JPO&INPIT |