摘要 |
PROBLEM TO BE SOLVED: To provide tissue paper which has smoothness and moist feeling equal to or better than those of conventional moisturized tissue paper and has reduced sticky feeling and reduced occurrence of tearing during use, and to provide a tissue paper product which does not tear easily when being pulled out.SOLUTION: In two-ply chemical-coated tissue paper, a chemical is applied so that the amount of the chemical contained in both surfaces is 1.5-5.5 g/m, and the basis weight per layer of sheets constituting the two-ply paper is 10-25 g/mand the thickness of the two-ply paper is 100-141 μm. A static friction coefficient in a lateral direction of a film and a static friction coefficient in a direction of pulling out a sheet of the tissue paper surface are 0.20-0.28. |