摘要 |
A high-toughness low-alloy wear-resistant steel sheet and a method of manufacturing the same, which has the chemical compositions (wt%): C: 0.08-0.20%; Si: 0.10-0.60%; Mn: 1.00-2.00%; B: 0.0005-0.0040%; Cr: less than or equal to 1.50%; Mo: less than or equal to 0.80%; Ni: less than or equal to 1.50%; Nb: less than or equal to 0.080%; V: less than or equal to 0.080%; Ti: less than or equal to 0.060%; Al: 0.010-0.080%, Ca: 0.0010-0.0080%, N: less than or equal to 0.0080%, O: less than or equal to 0.0080%, H: less than or equal to 0.0004%, P: less than or equal to 0.015% , S: less than or equal to 0.010% , and (Cr/5+Mn/6+50B): more than or equal to 0. 20% and less than or equal to 0.55%; (Mo/3+Ni/5+2Nb): more than or equal to 0.02% and less than or equal to 0.45%; (Al+Ti): more than or equal to 0.01% and less than or equal to 0.13%, the remainders being Fe and unavoidable impurities. The present invention reduces the contents of carbon and alloy elements, and makes full use of the charactristics of refinement, strengthening, etc. of micro-alloy elements such as Nb, Ti, etc., and through TMCP process, the wear-resistant steel sheet has high strength, high hardness, good toughness, good weldability, excellent wear-resistant performance, and is applicable to wearing parts in various mechanical equipments. |