发明名称 METHODS AND APPARATUS FOR FABRICATING AND CUTTING FLEXIBLE GLASS AND POLYMER COMPOSITE STRUCTURES
摘要 Methods and apparatus provide for: sourcing an ultra-thin glass sheet having first and second opposing major surfaces and perimeter edges therebetween, the glass sheet having a thickness between the first and second surfaces of less than about 400 microns; adhering at least one polymer layer directly or indirectly to at least one of the first and second surfaces of the glass sheet to form a laminated structure; and cutting the laminated structure using at least one of the following techniques: shear cutting, burst cutting, slit cutting, and crush cutting.
申请公布号 US2016023448(A1) 申请公布日期 2016.01.28
申请号 US201414774469 申请日期 2014.03.10
申请人 CORNING INCORPORATED 发明人 Bookbinder Dana Craig;Cimo Patrick Joseph;Gopalakrishnan Karthik;Gross Timothy Michael;Guerrero-Medina Glafiro;Kang Kiat Chyai;Lewis Sue Camille
分类号 B32B43/00;B32B17/10 主分类号 B32B43/00
代理机构 代理人
主权项 1. A method, comprising: sourcing an ultra-thin glass sheet having first and second opposing major surfaces and perimeter edges therebetween, the glass sheet having a thickness between the first and second surfaces of less than about 400 microns; adhering at least one polymer layer directly or indirectly to at least one of the first and second surfaces of the glass sheet to form a laminated structure; and cutting the laminated structure using at least one of the following techniques: shear cutting, burst cutting, slit cutting, and crush cutting, wherein the cutting step produces at least one cut edge having an edge characteristic in which lateral cracks running from the cut edge into the glass sheet penetrate no further than one of: (i) about 1400 microns; (ii) about 1000 microns; (iii) about 800 microns; (iv) about 600 microns; and (v) about 400 microns; (vi) about 200 microns; (vii) about 100 microns, and (viii) about 50 microns.
地址 Corning NY US