发明名称 Method for producing a bearing ring
摘要 A method for producing a bearing ring of a rolling bearing includes the steps of: preparing a formed body constituted of hypereutectoid steel; forming an annular heated region heated to a temperature of at least an A1 point on the formed body by relatively rotating an induction heating member arranged to face part of an annular region for becoming a rolling contact surface of the bearing ring in the formed body to induction-heat the formed body along the circumferential direction of the annular region; and simultaneously cooling the whole of the heated region to a temperature of not more than an Ms point.
申请公布号 US9243305(B2) 申请公布日期 2016.01.26
申请号 US201213980834 申请日期 2012.01.12
申请人 NTN CORPORATION 发明人 Yuki Hiroshi;Ohki Chikara;Yagita Kazuhiro
分类号 C21D9/40;F16C33/64;C21D1/10;C21D1/28;C21D1/30;C22C38/00;F16C23/08;C21D1/18;C21D1/19 主分类号 C21D9/40
代理机构 McDermott Will & Emery LLP 代理人 McDermott Will & Emery LLP
主权项 1. A method for producing a bearing ring of a rolling bearing, comprising the steps of: preparing a formed body constituted of hypereutectoid steel; forming an annular heated region heated to a temperature of at least an A1 point on said formed body by relatively rotating an induction heating member arranged to face part of the annular region of said formed body for becoming a rolling contact surface of said bearing ring in said formed body to induction-heat said formed body along a circumferential direction of said annular region, wherein said formed body is retained at a temperature of 850° C. to 900° C. for a period of time greater than 10 seconds; and simultaneously cooling a whole of said annular heated region to a temperature of not more than an Ms point, wherein in the step of cooling the whole of said annular heated region, the temperature of said annular heated region is retained within a range of predetermined temperature and time in which an area ratio of carbide in said rolling contact surface becomes at least 5.2% and a hardness of said rolling contact surface becomes at least 62 HRC after the whole of said annular heated region is cooled, and thereafter, the whole of said annular heated region is cooled.
地址 Osaka JP