发明名称 |
Resin injection molding method and resin injection molded product |
摘要 |
A resin injection molding method of molding a resin by injection-filling an inside of a mold cavity formed by mold-clamping a pair of a design surface mold and a non-design surface mold, with a melted thermoplastic polypropylene resin composition, the method including: setting a temperature of each cavity-forming surface of the design surface mold and the non-design surface mold prior to the injection filling to 60° C. to 120° C., with the temperature of the cavity-forming surface of the design surface mold being 5° C. to 50° C. higher than the temperature of the cavity-forming surface of the non-design surface mold; and causing the resin pressure to reach a negative pressure within 7 seconds after injection filling is complete, wherein the thermoplastic polypropylene resin composition contains a crystalline polypropylene resin and a rubber component and a content of the rubber component is 1 mass % to 40 mass %. |
申请公布号 |
US9242400(B2) |
申请公布日期 |
2016.01.26 |
申请号 |
US201314408473 |
申请日期 |
2013.06.20 |
申请人 |
Kumi Kasei Co., Ltd.;UBE MACHINERY CORPORATION, LTD. |
发明人 |
Fujita Yoshikazu;Imai Yoshiaki;Okahara Etsuo |
分类号 |
B29C45/73;B29C45/00;C08L23/12;B29K23/00;B29K21/00;B29L31/00 |
主分类号 |
B29C45/73 |
代理机构 |
Kolisch Hartwell, P.C. |
代理人 |
Kolisch Hartwell, P.C. |
主权项 |
1. A resin injection molding method of molding a resin by injection-filling an inside of a mold cavity, which is formed by mold-clamping a pair of design surface mold and non-design surface mold, with a melted thermoplastic polypropylene resin composition, the method comprising:
setting a temperature of each of cavity-forming surfaces of the design surface mold and the non-design surface mold prior to the injection filling to 60° C. to 120° C., and setting the temperature of the cavity-forming surface of the design surface mold to be higher than the temperature of the cavity-forming surface of the non-design surface mold by 5° C. to 50° C., and causing the resin pressure to reach to a negative pressure within 7 seconds after completion of the injection filling of the thermoplastic polypropylene resin composition, wherein the thermoplastic polypropylene resin composition contains a crystalline polypropylene resin and a rubber component and a content of the rubber component is 1 mass % to 40 mass %. |
地址 |
JP |