发明名称 Multicoat Coating With A Primer-Surfacer Coat Of A Nonaqueous Coating Material Comprising At Least Two Different Polyesters
摘要 Method for producing a multicoat coating comprises: applying a primer-surfacer coat (I) to an optionally pretreated substrate, curing coat (I), applying a basecoat (II) to coat (I), optionally curing the basecoat (II), applying a clearcoat (III) to basecoat (II), and curing basecoat (II) and/or clearcoat (III), wherein coat (I) is obtained by applying a nonaqueous, solventborne coating material comprising by weight: at least 20% of at least one organic solvent, at least 8% of at least one first polyester (A1), having a glass transition temperature of at least 20° C. and an acid number of 0 to 40 mg KOH/g; at least 8% by weight of at least one second polyester (A2), different from (A1) and having a glass transition temperature of not more than 10° C.; at least one crosslinker (B); and at least 8% of one or more fillers and/or pigments (C).
申请公布号 US2016017176(A1) 申请公布日期 2016.01.21
申请号 US201314379912 申请日期 2013.02.20
申请人 BASF Coatings GmbH 发明人 Wonnemann Heinrich
分类号 C09D167/02;B05D7/00;B05D1/02 主分类号 C09D167/02
代理机构 代理人
主权项 1. A method for producing a multicoat coating comprising: i) applying a primer-surfacer coat (I) to an optionally pretreated substrate, ii) curing the primer-surfacer coat (II), iii) applying a basecoat (II) to the cured primer-surfacer coat (I), iv) optionally curing the basecoat (II), v) applying a clearcoat (III) to the cured or uncured basecoat (II), and vi) curing the clearcoat (III) or the basecoat and the clearcoat if the basecoat was not cured in step iv), wherein the primer-surfacer coat (I) is obtained by applying a nonaqueous, solventborne coating material (F) comprising at least 20% by weight, based on the total coating material (F), of at least one organic solvent, and alsoA1) at least 8% by weight, based on the total coating material (F), of at least one first polyester (A1), having a glass transition temperature of at least 20° C. and an acid number of 0 to 40 mg KOH/g,A2) at least 8% by weight, based on the total coating material (F), of at least one second polyester (A2), different from (A1) and having a glass transition temperature of not more than 10° C.,B) at least one crosslinker (B), andC) at least 8% by weight, based on the total coating material (F), of one or more fillers and/or pigments (C).
地址 Münster DE
您可能感兴趣的专利