发明名称 FIRST-LAYER SUBMERGED ARC WELDING METHOD FOR HIGH-Cr CSEF STEEL
摘要 A submerged arc welding method for high-Cr creep strength-enhanced ferritic (CSEF) steel is provided which is capable of inhibiting the formation of hot cracks in a first layer, without increasing the number of steps and the amount of work. The present invention is characterized in that a metal powder or cut wire (21f) which includes not more than 0.10 mass% of C, not more than 0.50 mass% of Si, not more than 1.50 mass% of Mn, not more than 0.025 mass% of P, and not more than 0.025 mass% of S, the remainder comprising Fe and unavoidable impurities, is used to fill a groove in a base metal (10) to a dispersion height (h) of 1.0-4.0 mm, and first-layer welding is performed. In the first-layer welding, a reduction in the melting point of the welded metal is inhibited by the metal powder (21f) or the like, and thus hot cracks can be inhibited.
申请公布号 WO2016010122(A1) 申请公布日期 2016.01.21
申请号 WO2015JP70436 申请日期 2015.07.16
申请人 KABUSHIKI KAISHA KOBE SEIKO SHO (KOBE STEEL, LTD.) 发明人 YAMASHITA, KEN;IKAI, KAZUYA
分类号 B23K35/30;B23K9/18;B23K9/23;B23K35/362 主分类号 B23K35/30
代理机构 代理人
主权项
地址