发明名称 室温硬化性ポリオルガノシロキサン組成物
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a room temperature-curable polyorganosiloxane composition which has satisfactory surface curing property, and is excellent in adhesiveness, particularly, in adhesion durability at high temperature and high humidity. <P>SOLUTION: The composition contains: 100 pts.wt. of (A) a polyorganosiloxane mixture composed of (A1) a polyorganosiloxane blocked with trialkoxysilyl groups at both terminals and (A2) a polyorganosiloxane blocked with dialkoxysilyl groups at both terminals, the ratio of the number of bifunctional silyl groups at terminals in the component (A2) to the total number of functional silyl groups at terminals in the component (A) being 40-80 mol%; 1-50 pts.wt. of (B) diorganopolysiloxane; 1-300 pts.wt. of (C) an inorganic filler; 0.5-15 pts.wt. of (D) alkoxysilane or a partial hydrolytic condensate thereof; 0.1-10 pts.wt. of (E) a titanium chelate catalyst; and 0.01-5 pts.wt. of (F) a tackifier. <P>COPYRIGHT: (C)2013,JPO&INPIT</p>
申请公布号 JP5839463(B2) 申请公布日期 2016.01.06
申请号 JP20110275312 申请日期 2011.12.16
申请人 モメンティブ・パフォーマンス・マテリアルズ・ジャパン合同会社 发明人 森田 康仁;飯田 勲
分类号 C08L83/06;C08K3/00;C08K5/5415;C08K5/544 主分类号 C08L83/06
代理机构 代理人
主权项
地址