摘要 |
<P>PROBLEM TO BE SOLVED: To provide a coating solution for forming an ink-acceptive film which is suitably used for the manufacture of a wiring material through a process to print a metallic paste or an ink containing a metallic nanoparticle on a base and calcine the metallic paste or the ink. <P>SOLUTION: This coating liquid for forming an ink-acceptive film contains discretely: (1) a mixed solution for forming a primary coat which contains a flocculate particle-containing product (A) including 25 to 100 mass% flocculant particle composed of not less than two primary particles, bound together, of a primary particle which is formed of at least, one kind selected from the group consisting of silica, titania, zirconia and alumina and of an average particle diameter ranging from 2 to 200 nm, and a condensation product (C) obtained by hydrolysis/condensation-reacting a special alkoxide compound; and (2) a mixed solution for forming a top coat including a metallic oxide particle (B) which is composed of at least, one kind selected from the group consisting of the silica, titania, zirconia and alumina and of a larger average particle diameter than that of the primary particle constituting the flocculant particle and the condensation product (C). <P>COPYRIGHT: (C)2009,JPO&INPIT |