摘要 |
Systems and methods for forming a spray-on insulation (SOFI) coating on a structure include providing a resin material and an isocyanate material, both maintained at a temperature of between approximately 95 and 105° F., and mixing the resin material and the isocyanate material to produce a mixed material (e.g., using a spray gun having a mixing module). Using a repeated overlapping pattern having a periodicity of between approximately 5 to 10 inches, the mixed material on the structure is sprayed using a spray profile that is substantially flat and is produced at a predetermined spray distance between approximately 25-40 inches. A non-ozone-depleting blowing agent may be used.
|