摘要 |
<p>The object of the invention is s a dry composite for the production of indoor decorative mortar, which contains 80...90 mass% of 00-type stone grind as filling material, 7...9 mass% of 1-6 mm diameter crushed stone or plastic granules as a structure creating material, 1...2.5 mass% cellulose based adhesive as an adhesive material, and as a further additive material 3.5... 4.5 mass% of damping granules of 0.5 -1 mm in diameter. Furthermore, the object of the invention is a method for the production of indoor decorative finishing mortar, primarily by using the composite according to the invention, in the course of which a 100 mass portion of dry composite is mixed into 25 mass portion of water, and the aqueous mixture so produced is allowed to stand for 30 minutes, then another 2 mass portion of water, calculated to the mass of the mortar, is mixed to the decorative mortar, then the mixture so produced is mixed again after 10...180 minutes of standing. The indoor skin mixed for application can be applied with a stainless sleeker.</p> |