摘要 |
FIELD: textile industry. ^ SUBSTANCE: treatment is carried out with composition, which contains the following components in wt parts: 20 borate of methyl phosphite, 1.3 of triethanolamine, 80 of water and 0.20-0.65 of 1% water solution of carboxymethylcellulose at 20C for 1 min. Fibres are dried on air and thermostatted at 100C for 30 min. ^ EFFECT: improved fire-resistance, water-resistance, strength and resistance to thermal-oxidative destruction of polyamide fibres, increased strength of polyamide cord joint to rubber on the basis of chloroprene rubber. ^ 2 tbl, 3 ex |