摘要 |
FIELD: explosives. ^ SUBSTANCE: invention is related to the field of solid propellant charge (SPC) making of ballistite type. Method for production of solid propellant charge of ballistite type, which contains technical carbon, includes mixing of fuel components, squeezing, rolling, drying and pressing of charge by stage method with application of shape-generating press-tool. Technical carbon is used in granulated form. Rolling of fuel is executed at the temperature of working roller of 65Ç105C, idle roller temperature of 50Ç90C and with thickness of fuel web of 1.3Ç4.0 mm. ^ EFFECT: invention provides for improvement of sanitary-hygienic conditions of SPC production and reduced technological losses of carbon. ^ 1 dwg, 1 tbl |