摘要 |
A thermoplastic resin comprising a block copolymer or a graft copolymer possessing (A) a crystalline hydrogenated norbornene ring-opening polymer unit and (B) a non-crystalline polymer unit having a glass transition temperature of 40 to 300° C.; A method for producing thermoplastic resin comprising hydrogenating a block copolymer or a graft copolymer possessing a norbornene ring-opening polymer unit (C) and a polymer unit (D) which is converted into the above-mentioned non-crystalline polymer unit (B) after hydrogenation, in the presence of a hydrogenation catalyst; and a molding material comprising the thermoplastic resin are provided. The thermoplastic resin of the present invention excels in transparency, heat resistance, and mechanical strength.
|