摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a transparent conductive laminate improved in its transparency, and scratch resistance and bending resistance of a conductive thin film in a transparent conductive thin film using a film base material, and also improved in pen input durability for use as a touch panel. <P>SOLUTION: The transparent conductive laminate is formed by laminating a first transparent dielectric thin film 2, a second transparent dielectric thin film 3 and a transparent conductive thin film 4 in this order on one face of the transparent film base material 1 with a thickness of 2-120μm, and laminating a transparent substrate 6 on the other face of the film base material through an adhesive layer 5. When setting the refractive index of light of the film base material 1 as n<SB>1</SB>, the refractive index of light of the first dielectric thin film 2 as n<SB>2</SB>, the refractive index of light of the second dielectric thin film 3 as n<SB>3</SB>and the refractive index of light of the conductive thin film 4 as n<SB>4</SB>, a relationship of n<SB>3</SB><n<SB>2</SB>≤n<SB>1</SB><n<SB>4</SB>is satisfied. <P>COPYRIGHT: (C)2009,JPO&INPIT</p> |