发明名称 METHOD FOR PRODUCING NON-ORIENTED MAGNETIC STEEL SHEET HAVING HIGH MAGNETIC FLUX DENSITY
摘要 <P>PROBLEM TO BE SOLVED: To provide a method for producing a non-oriented magnetic steel sheet which can obtain a high magnetic flux density at low cost. <P>SOLUTION: In the production of the non-oriented magnetic steel sheet satisfying 0.1-2.0% Si, &le;1.0% Al and 0.1-2.0% Si+2Al and containing &le;0.004% C, it is decided that a slab heating temperature ST in a hot-rolling is 700-1,150&deg;C, a finish-rolling starting temperature FOT is 650-850&deg;C and a finish hot-rolling completing temperature FT is 550-800&deg;C. <P>COPYRIGHT: (C)2011,JPO&INPIT
申请公布号 JP2011111658(A) 申请公布日期 2011.06.09
申请号 JP20090270477 申请日期 2009.11.27
申请人 NIPPON STEEL CORP 发明人 KAWAMATA RYUTARO;KUBOTA TAKESHI
分类号 C21D8/12;B21B3/02;C22C38/00;C22C38/06;H01F1/16;H01F27/245 主分类号 C21D8/12