发明名称 processos de tratamento de uma escària bruta de aciaria para transformÁ-la em um ligante hidrÁulico pelo menos equivalente a um clÍnquer de cimento portland e de obtenÇço, a partir de uma escària de aciaria, de um ligante hidrÁulico equivalente a um cimento portland.
摘要 <p>A method for treating a raw steel plant slag to transform it into a hydraulic binder at least equivalent to a Portland cement clinker, comprises the following steps: oxidizing treatment with input of oxygen, air or a mixture thereof at a pressure ranging between 1 to 15 bars, at a temperature ranging between 1650 and 1400° C., of raw steel slag containing, relative to the raw slag total weight, at least 45 wt. % of CaO and less than 30 wt. % of Fe<SUB>2</SUB>O<SUB>3</SUB>; and adding to the slag a lime source optionally with silica and/or alumina, so that the slag, after tranformation and at room temperature, has a propotion of Fe<SUB>2</SUB>O<SUB>3 </SUB>of less than 13 wt. % and a mineralogical composition comprising at least 40 wt. % in C<SUB>3</SUB>S mineralogical phase and more than 10 wt. %, of calcium ferrite, relative to the final slag total weight.</p>
申请公布号 BR0206959(B1) 申请公布日期 2010.12.14
申请号 BR20020206959 申请日期 2002.02.01
申请人 发明人 VALERIE MICHAUD POUPARDIN;FRANCOIS SORRENTINO
分类号 C04B5/06;C04B7/153;C04B7/17;C04B7/21;C04B18/14;C21C1/02;C21C5/28;F27D15/00 主分类号 C04B5/06
代理机构 代理人
主权项
地址