摘要 |
<p>The present invention relates to a biaxially oriented polypropylene film containing: a polypropylene resin as a main component thereof, having a weight average molecular weight of 100,000 or more and 500,000 or less, the weight average molecular weight being determined by gel permeation chromatography, wherein at least one surface of the biaxially oriented polypropylene film has a protrusion volume of 2.0×104 μm3 or more and 3.0×104 μm3 or less, the protrusion volume being determined in an area of 560 μm×745 μm using a super-depth surface profile measurement microscope by determining an average plane of the surface based on distances between plural points on the surface and an irradiation source of the super-depth surface profile measurement microscope and measuring a volume of protrusions projecting from the average plane.</p> |