发明名称 Recording film for optical information recording medium, optical information recording medium, and sputtering target used to form said recording film
摘要 Provided is a recording film for an optical information recording medium with which it is possible to meet all predetermined characteristics requirements and increase productivity while reducing the number of layers in the optical information recording medium. The present invention relates to a recording film for an optical information recording medium on which recording is performed by laser light irradiation, wherein the recording film for an optical information recording medium includes: Mn; at least one element (group X element) selected from the group consisting of Bi, Ag, Co, Cu, In, Sn, and Zn (group X); and oxygen (O). At least some of the Mn and at least some of the group X element are oxidized.
申请公布号 US9214181(B2) 申请公布日期 2015.12.15
申请号 US201214115547 申请日期 2012.05.30
申请人 Kobe Steel, Ltd. 发明人 Shida Yoko;Tauchi Yuki
分类号 G11B7/24;G11B7/243;C23C14/00;C23C14/08;C23C14/34 主分类号 G11B7/24
代理机构 Oblon, McClelland, Maier & Neustadt, L.L.P. 代理人 Oblon, McClelland, Maier & Neustadt, L.L.P.
主权项 1. A recording film, comprising: Mn; one or more X elements; and oxygen; wherein the one or more X elements satisfy one of conditions (A) to (E): (A) the one or more X elements are Cu, and, based on a total amount of Mn and Cu, an atomic proportion of Mn is more than 10% and 80% or less,(B) the one or more X elements are Bi and Cu, and, based on a total amount of Mn, Bi and Cu, an atomic proportion of Bi is 10% or more and 50% or less, and an atomic proportion of Mn is 20% or more and 40% or less,(C) the one or more X elements are Bi and In, and, based on a total amount of Mn, Bi and In, an atomic proportion of Bi is 20% or more and less than 40%, and an atomic proportion of In is more than 20% and 40% or less,(D) the one or more X elements are Ag and In, and, based on a total amount of Mn, Ag and In, an atomic proportion of Mn is 30% or more and 50% or less, and an atomic proportion of In is 30% or more and 50% or less, and(E) the one or more X elements are Bi, Cu and Co, and, based on a total amount of Mn, Bi, Cu and Co, an atomic proportion of Mn is 20% or more and 40% or less, an atomic proportion of Cu is 10% or more and 35% or less, and an atomic proportion of Bi is 10% or more and 30% or less; the recording film is suitable for an optical information recording medium recordable by irradiation with a laser ray; and at least part of Mn and part of the one or more X elements are oxidized.
地址 Kobe-shi JP