发明名称 NONAQUEOUS ELECTROLYTE SECONDARY BATTERY AND MANUFACTURING METHOD OF THE SAME
摘要 A manufacturing method according to the present invention includes: preparing a positive-electrode active material including sulfate ions by 0.04 mmol/m2 to 0.16 mmol/m2 per unit specific surface area; manufacturing a positive electrode by use of the positive-electrode active material including sulfate ions; manufacturing a negative electrode by use of a negative-electrode active material; assembling a battery assembly by accommodating the positive electrode, the negative electrode, and a nonaqueous electrolyte including lithium difluoro bis-oxalate phosphate in a battery outer case, wherein an additive amount (μmol) of the lithium difluoro bis-oxalate phosphate in the nonaqueous electrolyte is determined so as to satisfy Formula (I); and performing a charging process on the battery assembly at least once.
申请公布号 US2015357678(A1) 申请公布日期 2015.12.10
申请号 US201514729427 申请日期 2015.06.03
申请人 TOYOTA JIDOSHA KABUSHIKI KAISHA 发明人 TSUBOUCHI Hiroshi
分类号 H01M10/0567;H01M10/0525 主分类号 H01M10/0567
代理机构 代理人
主权项 1. A method for manufacturing a nonaqueous electrolyte secondary battery, the method comprising: preparing a positive-electrode active material including sulfate ions by not less than 0.04 mmol/m2 but not more than 0.16 mmol/m2 per unit specific surface area; manufacturing a positive electrode by use of the positive-electrode active material including sulfate ions; manufacturing a negative electrode by use of a negative-electrode active material; assembling a battery assembly by accommodating the positive electrode, the negative electrode, and a nonaqueous electrolyte including lithium difluoro bis-oxalate phosphate in a battery outer case, wherein an additive amount X (μmol) of the lithium difluoro bis-oxalate phosphate in the nonaqueous electrolyte is determined so as to satisfy the following formula (I):0.004≦X(Sc·Wc+Sa·Wa)≦0.037(I)(in the formula (I), Sc indicates a specific surface area (m2/g) of the positive-electrode active material, We indicates a mass (g) of the positive-electrode active material, Sa indicates a specific surface area (m2/g) of the negative-electrode active material, and Wa indicates a mass (g) of the negative-electrode active material); and performing a charging process on the battery assembly at least once, so as to form films on surfaces of the positive-electrode active material and the negative-electrode active material.
地址 Toyota-shi JP