发明名称 High resistance gray iron alloy for combustion engines and general casts
摘要 The object of this application defines a new alloy which presents at the same time the mechanical and physical properties of the gray iron alloy, i.e., excellent machinability, damping vibration, thermal conductivity, low shrink tendency and good microstructure stability, together with a wide interface range of the CGI tensile strength.
申请公布号 US9200351(B2) 申请公布日期 2015.12.01
申请号 US200913201337 申请日期 2009.02.12
申请人 TEKSID DO BRASIL LTDA. 发明人 Mol de Oliveira Otto Luciano;Villafort Jefferson Pinto
分类号 C22C37/06;C22C37/00;C22C37/10 主分类号 C22C37/06
代理机构 Volpe and Koenig, P.C. 代理人 Volpe and Koenig, P.C.
主权项 1. A high resistance gray iron alloy comprising, in weight, iron and C in an amount of 2.8% to 3.2%; Si in an amount of 2.0% to 2.40%; Mn in an amount of 0.4% to 0.5% and S in an amount defined in specific ranges by a ratio Mn/S: when Mn is 0.40% Mn/S is 3.3 to 3.9when Mn is 0.47% Mn/S is 4.0 to 5.0;when Mn is 0.50% Mn/S is 4.9 to 6.0; Cr in an amount of 0.4% maximum and dependent upon an amount of Mo, wherein Cr+Mo is less than or equal to 0.65%; Sn and Cu in amounts satisfying 0.010% <Cu/10+Sn<0.021%; and P in an amount of 0.01% maximum;wherein the alloy has the following properties:Heat Transfer Rate (W/m °K):  45 to 60Hardness (HB) 230 to 250Tensile Strength (Mpa) 300 to 370Fatigue Strength (Mpa): By 170 to 190Rotating BandingThermal Fatigue (Cycles): Temperature20 × 103Range 50° c.-600° c.Machinability (Km): Milling By  9 to 11Ceramic Tool At 400 m/Min Speed:Micro Structurepearlite 98-100%; graph A, 4/7Shrinkage Tendency (%) 1.0 to 2.0Damping Factor (%):  90 to 100Poisson's Rate: At Room Temperature0.25 to 0.27
地址 Betim/Mg BR