发明名称 |
Floating seal |
摘要 |
A floating seal comprises C, Si, Mn, Ni, Cr, Mo, V, and B with the remainder being made up of Fe and unavoidable impurities. The contents of the C, Si, Mn, Ni, Cr, Mo, V and B are C: 2.2 to 3.9 wt %, Si: 0.5 to 3.5 wt %, Mn: 0.1 to 2.0 wt %, Ni: 0.5 to 4.3 wt %, Cr: 7.5 to 25.0 wt %, Mo: 0 to 8.0 wt % (excluding 0 %), V: 0 to 6.0 wt % (excluding 0%), and B: 0.02 to 0.4 wt %. The content of Cr in the parent phase is 2.00 to 5.41 wt %. The content of graphite is 0.05 to 0.35% of the surface area. The content of carbon boride is 19 to 40% of the surface area. |
申请公布号 |
US9200710(B2) |
申请公布日期 |
2015.12.01 |
申请号 |
US201214355965 |
申请日期 |
2012.09.27 |
申请人 |
KOMATSU LTD. |
发明人 |
Nishioka Masato |
分类号 |
F16J15/34 |
主分类号 |
F16J15/34 |
代理机构 |
Global IP Counselors, LLP |
代理人 |
Global IP Counselors, LLP |
主权项 |
1. A floating seal comprising C, Si, Mn, Ni, Cr, Mo, V, and B with a remainder being made up of Fe and unavoidable impurities, wherein the the floating seal contains C, Si, Mn, Ni, Cr, Mo, V, and B in amounts as follows:
C: 2.2 to 3.9 wt % Si: 0.5 to 3.5 wt % Mn: 0.1 to 2.0 wt %; Ni: 0.5 to 4.3 wt %; Cr: 7.5 to 25.0 wt %; Mo: greater than 0 to 8.0 wt %; V: greater than 0 to 6.0 wt %; B: 0.02 to 0.4 wt %; and a content of Cr in a parent phase is 2.00 to 5.41 wt %; a content of graphite is 0.05 to 0.35% of a surface area of the floating seal, and a content of carbon boride is 19 to 40% of the surface area. |