发明名称 |
Piston ring having a thermally sprayed coating and method for producing same |
摘要 |
A method for producing a piston ring for an internal combustion engine includes providing, a substrate and applying a coating by means of thermal spraying of a powder including solid lubricants on the substrate, having the elemental proportions of 15-30% by weight of iron, Fe; 15-30% by weight tungsten, W; 25-35% by weight of chromium, Cr; 10-35% by weight of nickel, Ni; 1-5% by weight of molybdenum, Mo; 0.2-3% by weight of aluminum, Al; 3-20% by weight of copper, Cu; 1-10% by weight of carbon, C; 0.1-2% by weight of sulfur, S; and 0.1-2% by weight of silicon, Si. The resultant piston ring and coating are also provided. |
申请公布号 |
US9194492(B2) |
申请公布日期 |
2015.11.24 |
申请号 |
US201113811582 |
申请日期 |
2011.06.20 |
申请人 |
Federal-Mogul Burscheid GmbH |
发明人 |
Kennedy Marcus;Zinnabold Michael;Matz Marc-Manuel |
分类号 |
B22F1/00;F16J9/26;B22F3/115;B22F5/10;C22C33/02;C23C4/06;C22C30/02;C09D1/00 |
主分类号 |
B22F1/00 |
代理机构 |
Dickinson Wright, PLLC |
代理人 |
Stearns Robert L.;Dickinson Wright, PLLC |
主权项 |
1. A spray powder for thermal spraying, wherein the powder, including a proportion of 5-20% by weight of solid lubricant, comprises the element proportions:
15-30% by weight of iron, Fe; 15-30% by weight of tungsten, W; 25-35% by weight of chromium, Cr; 10-35% by weight of nickel, Ni; 1-5% by weight of molybdenum, Mo; 0.2-3% by weight of aluminium, Al; 3-20% by weight of copper, Cu; 1-10% by weight of carbon, C; 0.1-2% by weight of sulphur, S; and 0.1-2% by weight of silicon, Si. |
地址 |
Burscheid DE |