发明名称 Drawing process for titanium
摘要 A cold drawing process for forming titanium blanks into titanium pieces in which the titanium blank is pre-treated with a wet lubricant prior to drawing. The wet lubricant lubricates the interfaces of the titanium blank and the punch to substantially reduce galling and hardening of the surface of the titanium blank from the drawing process, thereby eliminating the need to anneal the formed titanium pieces prior to additional drawing, stamping, punching or other forming processes.
申请公布号 US9192973(B1) 申请公布日期 2015.11.24
申请号 US201313801035 申请日期 2013.03.13
申请人 Meier Tool & Engineering, Inc. 发明人 VanDanacker Tony;Gehling Mike;Gaffaney Jordan;Klebs Corey;Diffley Jason;Olson Levi;Sportel Scott
分类号 B21D22/20 主分类号 B21D22/20
代理机构 Patterson Thuente Pedersen, P.A. 代理人 Patterson Thuente Pedersen, P.A.
主权项 1. A method of forming generally planar titanium blanks into formed titanium pieces comprising: providing a first die assembly comprising a first die defining a first recessed cavity and a first punch movable along a first linear path intersecting the first recessed cavity; providing a generally planar titanium blank having at least one roughened face; applying a wet lubricant to the roughened face of the titanium blank; positioning the titanium blank on the first die such that a portion of the titanium blank is aligned with the first recessed cavity of the first die; moving the first punch along the first linear path to engage the lubricated roughened face of the titanium blank and deform the aligned portion of the titanium blank into the first recessed cavity of the first die; providing a second die assembly comprising a second die defining a second recessed cavity and a second punch movable along a second linear path intersecting the second recessed cavity; applying additional wet lubricant to the roughened face of the formed titanium piece; positioning the formed titanium piece on the second die such that deformed portion of the titanium blank is received within the second recessed cavity of the second die; and moving the second punch along the second linear path to engage the lubricated roughened face of the titanium blank and elongate the deformed portion of the titanium blank.
地址 Anoka MN US