发明名称 表面処理方法
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a surface treatment method for covering the surface of a member to be treated with a water/oil repellent film having excellent durability. <P>SOLUTION: A steel plate heated to 80°C is immersed in a solution A which contains tetraethoxysilane, water, ethanol, and silica particles whose average primary particle size is 30 nm and whose pH is adjusted to 3.0 by hydrochloric acid, and is pulled up. When the solution A evaporates, the steel plate is promptly put in a solution B (a sodium hydroxide aqueous solution of pH12) and is immersed for 30 minutes. On the surface of the steel plate, a silica film with an uneven surface is formed. The steel plate is immersed in a solution C which contains 1H, 1H, 2H, 2H-perfluoro decyltriethoxysilane, water and ethanol and whose pH is adjusted to 3.0 by hydrocholoric acid. The steel plate is pulled up after being immersed for 30 minutes, and is immersed in the solution B for 30 minutes. Then, the steel plate with a water/oil repellent layer formed on the silica film is obtained. <P>COPYRIGHT: (C)2013,JPO&INPIT</p>
申请公布号 JP5821567(B2) 申请公布日期 2015.11.24
申请号 JP20110258067 申请日期 2011.11.25
申请人 发明人
分类号 B05D3/02;B05D5/00;C09K3/18 主分类号 B05D3/02
代理机构 代理人
主权项
地址
您可能感兴趣的专利