摘要 |
PROBLEM TO BE SOLVED: To provide a polyacetal resin composition that reduces the amount of formaldehyde generated from a molded product and is also excellent in long-term property and moldability.SOLUTION: A polyacetal resin composition comprises polyacetal resin (A), and a compound (B) having alkali metal or alkaline earth metal, with the compound (B) having alkali metal or alkaline earth metal having a decomposition start temperature of 190°C or more. |