A method for forming a composition exhibiting energy dissipation in at least a portion of the frequency range from about 1 GHz to about 20 GHz can comprise treating a magnetic lossy material to increase the brittleness of the material, processing at least a portion of the magnetic lossy material into a powder, and mixing at least a portion of the powder with a dielectric resin, wherein the percentage volume of the powder relative to the total volume of the composition is configured such that dissipation of incident electromagnetic radiation is substantially optimized in at least a portion of the frequency range from about 1 GHz to about 20 GHz.
申请公布号
EP2944164(A2)
申请公布日期
2015.11.18
申请号
EP20140704414
申请日期
2014.01.11
申请人
SABIC GLOBAL TECHNOLOGIES B.V.
发明人
SIMONE, DAVIDE LOUIS;BALCH, GARY STEPHEN;GIBSON, DAVID ALEXANDER;PATCHEN, HAROLD JAY;GARNER, ALLEN LAWRENCE;PARKER, GREGORY JOHN;TAN, DANIEL QI;JOHNSON, FRANCIS