发明名称 R−T−B−M−C系焼結磁石の製造方法、及びその製造装置
摘要 The present invention refers to a method of manufacturing an R-T-B-M-C sintered rare earth magnet comprising the process steps of: a) charging an R-T-B-M-C alloy powder including a lubricant into a mold cavity with a predetermined density, wherein R is at least one rare earth element including Y and Sc, T is iron or a mixture of iron and cobalt, and M is at least one element selected from Ti, Ni, Nb, Al, V, Mn, Sn, Ca, Mg, Pb, Sb, Zn, Si, Zr, Cr, Cu, Ga, Mo, W and Ta, and the weight contents of these components are in the ranges 25 % ‰¤ R ‰¤ 40 %, 60 % ‰¤ T ‰¤ 74 %, 0 % ‰¤ M ‰¤ 2 %, 0.8 % ‰¤ B ‰¤ 1.2 %, 0.03 % ‰¤ C ‰¤ 0.15 %; b) applying a magnetic field to the powder filled in the mold cavity under a pressure in the range of 0.2 to 2 MPa; and c) sintering the same under inert gas followed by an additional heat treatment.
申请公布号 JP5815655(B2) 申请公布日期 2015.11.17
申请号 JP20130254679 申请日期 2013.12.10
申请人 煙台首鋼磁性材料株式有限公司 发明人 彭衆傑;劉暁通;崔勝利;丁開鴻
分类号 B22F3/02;B22F3/03;C22C33/02;C22C38/00;H01F1/057;H01F1/08;H01F41/02 主分类号 B22F3/02
代理机构 代理人
主权项
地址