摘要 |
PROBLEM TO BE SOLVED: To provide a method of manufacturing a hard coat film in which poor appearance is hardly caused in the manufacturing steps and which has a hard coat layer with sufficient hardness.SOLUTION: A hard coat film 10 comprises a base material film 1 and a hard coat layer 2 laminated on the top of at least one surface of the base material film 1. In the hard coat film 10, the hard coat layer 2 is formed of a coating liquid containing a compound having an energy polymerizable functional group, a filler, a polymerization initiator, and a polythiol compound. A proportion of a variation &Dgr;bof a value bof the chromatic coordinate bstipulated in JIS K5600-4-4:1999 (ISO 7724-1:1984) after applying a heat treatment of keeping the hard coat film 1 in a 200°C environment for one hour, with respect to a value bof the chromatic coordinate bof the hard coat film 1 before the heat treatment, to a total thickness of the hard coat layer is less than 0.02 μm. |