发明名称 |
METHOD OF PRODUCING OF MODIFIED ALUMINIUM ALLOYS |
摘要 |
FIELD: metallurgy.SUBSTANCE: molten aluminium alloy at the temperature 750÷800°C is added by cryolite powder NaAlF6 wt %, after the minimum time period 10 minutes the molten metal is added by modifier 5÷6 wt % at simultaneous activation of the molten metal within no less than 20 minutes by mechanical mixing and/or by ultrasonic oscillations at the frequency 10 kHz, and/or electromagnetic field with the frequency 40 Hz. The modifier is the mix mixed down to the uniform state consisting of nanopowder of 20 wt % titanium, 5 wt % carbon nanopowder and 75 wt % cryolite powder.EFFECT: increase of strength and wear resistance of the disperse strengthened alloys due to formation of in situ of nanoparticles of titanium carbide evenly distributed in the aluminium die.1 dwg, 1 ex |
申请公布号 |
RU2567779(C1) |
申请公布日期 |
2015.11.10 |
申请号 |
RU20140129130 |
申请日期 |
2014.07.15 |
申请人 |
OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOST'JU "ALIMINIEVYE KOMPOZITY" OOO "ALKOM" |
发明人 |
ARKHIPOV VLADIMIR AFANAS'EVICH;DAMMER VIKTOR KHRISTIANOVICH;VOROZHTSOV ALEKSANDR BORISOVICH;ZHUKOV ALEKSANDR STEPANOVICH;VOROZHTSOV SERGEJ ALEKSANDROVICH;ZHUKOV IL'JA ALEKSANDROVICH |
分类号 |
C22C1/10;B82Y30/00;C22C21/00 |