The present invention relates to a fabric production method for a skin scrubbing tool, which has increased resilence and detergency. To this end, a base yarn is produced by primarily twisting two strands of yarn fibers (y1, y2) of composite yarn fiber with 70-150 denier at 1,200-2,700 TPM in S or Z directions. (Z-direction is shown in the figure.) In addition, a total composite twisted yarn (S) is produced by secondarily composite-twisting two strands of base yarn fibers which are primarily twisted at 600-2,700 TPM in Z- or S-directions. (S-direction is shown in the figure.) and the composite twisted yarn (S) comprises a loop-shaped body by knitting the composite twisted yarn (S) with a knitting machine. |