摘要 |
<p>Disclosed are: a polybutylene terephthalate resin composition which is capable of providing a metal composite component having excellent adhesion between a metal component and the polybutylene terephthalate resin composition even in cases where the mold temperature is 100°C or less; and a method for producing a metal composite component. Also disclosed is a metal composite component which has excellent adhesion between a metal component and a polybutylene terephthalate resin composition. Specifically, a metal composite component is produced by blending a specific amount of a polyethylene terephthalate resin, which is modified by a dicarbonyl unit other than a terephthaolyl unit, into a polybutylene terephthalate resin.</p> |