发明名称 FERRITIC HEAT-RESISTANT STEEL, AND MANUFACTURING METHOD FOR SAME
摘要 There is provided a heat resistant ferritic steel including a base material including, by mass percent, C: 0.01 to 0.3%, Si: 0.01 to 2%, Mn: 0.01 to 2%, P: at most 0.10%, S: at most 0.03%, Cr: 7.5 to 14.0%, sol.Al: at most 0.3%, and N: 0.005 to 0.15%, the balance being Fe and impurities, and an oxide film that is formed on the base material and contains 25 to 97% of Fe and 3 to 75% of Cr. This heat resistant ferritic steel is excellent in photoselective absorptivity and oxidation resistance.
申请公布号 EP2784172(A4) 申请公布日期 2015.11.04
申请号 EP20120850846 申请日期 2012.11.21
申请人 NIPPON STEEL & SUMITOMO METAL CORPORATION 发明人 NISHIYAMA, YOSHITAKA;MATSUO, HIROSHI;OTSUKA, SHUNICHI
分类号 C23C8/18;C21D6/00;C22C38/00;C22C38/02;C22C38/04;C22C38/14;C22C38/18;C22C38/20;C22C38/22;C22C38/24;C22C38/26;C22C38/30;C22C38/38;C22C38/58;C23C4/10;C23C4/12 主分类号 C23C8/18